when I order a thermocouple wire for doing oven profiles, it... - Jul 20, 2006 by fordf1502004
based on experience, no significant change. ... - Jul 21, 2006 by Reypal
How do you plan on fusing the wires back together ? ... - Jul 21, 2006 by Sr. Tech
Cut the loose ends and not the couple? Russ ... - Jul 21, 2006 by RDR
The ones we use are sealed on the plug end. ... - Jul 21, 2006 by Sr. Tech
you can use a thermocouple welder to fuse the wires back. as... - Jul 21, 2006 by Amol Kane
Not to argue, but you can use a spot welder to fuse thermoco... - Jul 21, 2006 by davef
Addressing the issue "Will cutting change the readings?" Ver... - Jul 24, 2006 by nodlac