Hi all, I wonder if some of you have experience in use of dr... - Jul 31, 2006 by
We use 5744 with good results. It remains solid (granular) a... - Aug 01, 2006 by Steve Thomas
Be careful and review the MSDS sheets on any dross inhibitor... - Aug 02, 2006 by Steve
What is the name of the dross eliminator you are referring t... - Aug 07, 2006 by
I would be interested to see what Dross eliminators are avai... - Aug 08, 2006 by
You can find some interesting stuff regarding MS2 here in th... - Aug 08, 2006 by Steve Thomas
Hello all, just wanted to say that I've been using MS2 for 2... - Aug 08, 2006 by
John, What is the cost/litre? aj... ... - Aug 09, 2006 by
I paid $168/ liter for the leaded on my recent order of 24 l... - Aug 10, 2006 by
John, What about the machine? I understand that pumps nee... - Aug 11, 2006 by
You can contact Graphic Research and Brad Koor will tell you... - Aug 14, 2006 by Baer
We've just conducted an MS2 study, and we found very little ... - Aug 14, 2006 by
Hello everybody, My name is Jay Hardin and I'm the MS2 Appli... - Aug 17, 2006 by
hi aj, I am interested to know where do you get the solder s... - Aug 21, 2006 by
Pulsar Solder Saver: "The Solder Saver is a unique, handheld... - Aug 21, 2006 by davef
I have just finished a trial on the "Pulsar Solder saver Uni... - Aug 22, 2006 by
Dear Sir, We produce solder dross reducing Powder and wave ... - Sep 04, 2006 by
Just reading these comments are really interesting but very ... - Sep 07, 2006 by
Greg, can you share what is this metallic anti drossing agen... - Sep 25, 2006 by
Sorry Bert For some reason I'm not getting the Email noti... - Oct 04, 2006 by