Hi all,, I running SMQ230 solder paste with a time above ... - Feb 12, 2007 by
Does this meet the SMQ230 recommended time above liquidous? ... - Feb 12, 2007 by Real Chunks
Looks good at first glance. Couple of questions, though: ... - Feb 12, 2007 by
Tks for the answers,, My concern is about the intermetalic l... - Feb 12, 2007 by
250-260ish seems a little on the high side ? Depending on... - Feb 12, 2007 by
Campos, This is a direct reply I recieved from Indium, (tha... - Feb 13, 2007 by Darby
Hi Darby, Where did you get the info. that cooling rate i... - Feb 16, 2007 by Dirk Nuendyke
As I stated, the reply was direct from Indium, (thanks to Ri... - Feb 18, 2007 by Darby
Darby, thanks for the good info. I actually read an article... - Feb 19, 2007 by Dirk Nuendyke
That's why you have to read between the lines of any article... - Feb 19, 2007 by Real Chunks
Those guys didnt suggest you get in there and check did they... - Feb 22, 2007 by Loco
campos