Views: 2969
Hi all have anyone has experiance in SMT on fexible circu... - Feb 15, 2007 by vshan
vshan, Good Morning. I used to work for a flex house and... - Feb 15, 2007 by
I didn't pose the question -- but have some: As the substrat... - Feb 15, 2007 by Jim Z
Jim, In a previous life, we built some flex circuits for ... - Feb 15, 2007 by robgd3
Hi Chris Good Day!!!! well we are running flex panel(150... - Feb 15, 2007 by vshan
Hi Jim Good Day yes we are using a pallet bottom support ... - Feb 15, 2007 by vshan
Hi Rob and all the type of pallet we are using is durast... - Feb 15, 2007 by vshan
Hi Vshan, Have more pallets made, and don't stack them - ... - Feb 16, 2007 by Rob