Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 5084
Hi all, Are there special type bags which you need to use... - May 16, 2007 by aj
You want Moisture Barrier Bags (MBB). It is possible you ar... - May 16, 2007 by Stephen
Hi Stephen, What if you used an anti-stat bag with a des... - May 16, 2007 by Real Chunks
Moisture barrier bags are polymer coated foil so are nearly ... - May 16, 2007 by Steve Thomas
3.3.2.1 Moisture Barrier Bag (MBB) The moisture barrier bag ... - May 16, 2007 by Stephen
"I read a study a while back by IBM that showed too strong a... - May 16, 2007 by Steve Thomas
Oh sorry. Let me try again.... If I seal a desiccant in an... - May 16, 2007 by Real Chunks
For a day or a week probably. Possibly a month. But I"m sur... - May 16, 2007 by Stephen
"Usually people use the vacuum to remove air and then replac... - May 16, 2007 by aj
Can't you schedule the bake to coincide with the production ... - May 16, 2007 by Steve Thomas