Hi, friends Need your urgent help on bellow issue ....... ... - Apr 26, 2010 by sudhir
Sudhir, This part appears to have a lot of mass, thus it ma... - Apr 26, 2010 by A Very Frazzled Man
We are using QP fuzi m/c during the placement of comp. PCB... - Apr 30, 2010 by sudhir
We do a similar part on a Fuji IP3. Set table speed to low.... - Apr 30, 2010 by jdengler
I do agree with Jerry: you should apply more paste on it,... - May 02, 2010 by Jesus
Make sure that both lead frames are contacting the PCB pads ... - May 05, 2010 by brad
From looking at your images I would say it could be poor sol... - May 08, 2010 by aj