> Contact your distributor for the coating or > Humiseal directly. Humiseal has had a recent > issue with batches of 1B31. The specific problem > is lack of adhesion, which is what you have as > well. You need to find out if your batch # is one > of the affected batches. If so they will gladly > replace it with a good batch.
> Contact your distributor for the coating or > Humiseal directly. Humiseal has had a recent > issue with batches of 1B31. The specific problem > is lack of adhesion, which is what you have as > well. You need to find out if your batch # is one > of the affected batches. If so they will gladly > replace it with a good batch.
Dear Sir,
Thanks for your reply. actually by reducing the thickness of coating we rectified the problem...
reply »