Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2632
Dear All, I´m looking for a low temp solder paste with Lead.... - Nov 25, 2011 by Fco Teixeira
Sn43/Pb43/Bi14 is a low temperature leaded alloy that has be... - Nov 25, 2011 by davef