I have a small board in a 5x5 array. Thickness is .014"... - Apr 30, 2021 by ProcEng1
Thin FR4 can be routed with a CO2 laser with high quality re... - May 03, 2021 by CAPSE
Can you use a conventional router? For boards that small an... - May 03, 2021 by DWL
It's annoying, but, the last time I was faced with a similar... - May 11, 2021 by robgd3
Obviously the more expensive route, but have you considered ... - May 11, 2021 by Chris
Punch dies are also expensive, inflexible and the punches ne... - Jun 03, 2021 by SMTA-64386637 SMTA