Is anyone out there reworking the AMP BGA ziff sockets? AMP's recommendation is that it cannot be reworked. I have successfully reworked the 604 ball version of this socket, but I am having problems with the 603 ball version. I am using an Air-Vac with Smart Track and having problems getting the profile to work. Any thoughts would be appreciated. Thanks