It's unusual to use a horseshoe shaped pad for a 0805. Commonly when people want to reduce the paste volume to reduce solder balling, they print a "home plate" aperature.
We print paste 1:1 with the pad.
�IPC-7351 LP Wizard� is the library maintenance tool that is revolutionizing the way designers work. The IPC-7351 LP family tools can give you access to options that will allow you to quickly and easily browse your PCB land pattern library to locate, view, construct and verify the mechanics of your PCB library design. [ pcblibraries.com/IPC7351 ][ landpatterns.ipc.org/default.asp ]