Apr 07, 2011

Edgebonded CBGA

Edgebonded CBGA

After removal of underfilled BGA, underfill residues must be removed.

After removal of underfilled BGA, underfill residues must be removed.

Zymet Inc. has introduced a reworkable edgebond adhesive, UA-2605, that improves thermal cycle performance of CBGAs and plastic BGAs. In one trial, UA-2605 tripled the 0°C to +100°C performance of a CBGA, to nearly 2500 cycles. Previously, an underfill was needed to achieve this level of performance.

The edgebond adhesive is much easier to process than an underfill. When applying underfill, the board is preheated to facilitate capillary flow, and multiple dispense passes are used to deposit sufficient material. With UA-2605, only four beads of the adhesive are required, one at each corner (Figure 1). There is no need to preheat the board, no need to wait for underfill flow, no need for multiple dispensing passes.

Reworking an underfilled BGA is a time consuming and delicate task. Underfill residues (Figure 2) must be removed and, for fine pitch BGAs, the risk of pad damage is high. With UA-2605, BGA rework is simple and straightforward. The temperature is raised and the adhesive is scraped away; then, the BGA is reflowed and lifted from the board. Little site cleaning is necessary.


Zymet (http://www.zymet.com) is a manufacturer of microelectronic and electronic adhesives and encapsulants. Its products include die attach adhesives, substrate adhesives, UV curable glob top and cavity-fill encapsulants, and underfill encapsulants.

Feb 08, 2013 -

Zymet Announces Highly Crack Resistant Underfill for Thin, Flexible Assemblies, CN-1751-4

Jan 13, 2012 -

New Underfill from Zymet for 0.4-mm pitch POP's

Mar 17, 2010 -

Low CTE Reworkable Underfill for Superior Thermal Cycle Performance

Sep 17, 2009 -

Reworkable Underfill for Package-on-Package (POP)

Apr 27, 2004 -

Reworkable Underfill Encapsulant for BGA's

Sep 25, 2003 -

Reworkable Underfill Encapsulant for CSP's and BGA's

Jul 06, 2022 -

Offline PCBA Cleaning Machine HJS-7100,rosin flux, non-clean flux,water-soluble flux cleaning machine

Jul 05, 2022 -

Semiconductor Spray Cleaning Machine HJS-9700,Semiconductor Wafer Cleaning Machine HJS-9700

Jul 04, 2022 -

Pneumatic Stencil Cleaner HJS-9000II,dual chamber stencil cleaning machine

Jul 03, 2022 -

Electric Stencil Cleaner HJS-9500, SMT Electric Stencil Cleaner HJS-9500

Jul 01, 2022 -

Screen Cleaning Machine HJS-4600, SMT Screen Cleaning Machine HJS-4600

Jun 30, 2022 -

Electric Fixture Cleaning Machine HJS-6700, SMT pallet cleaning machine, soldering pallet cleaning machine

Jun 29, 2022 -

Waste Water Treatment Machine RWT-1000, SMT Waste Water Treatment Machine RWT-1000

Jun 28, 2022 -

Gen3's Dr Chris Hunt, CTO submits an insightful paper to the journal of Surface Mount Technology

Jun 28, 2022 -

Squeegee Cleaning Machine HJS-3700,SMT Squeegee Cleaning Machine HJS-3700

Jun 27, 2022 -

Solderstar Celebrates 20 Years of Innovation

See electronics manufacturing industry news »

Reworkable Edgebond Adhesive Improves CBGA and BGA Thermal Cycle Performance and Eliminates Underfill news release has been viewed 1543 times

  • SMTnet
  • »
  • Industry News
  • »
  • Reworkable Edgebond Adhesive Improves CBGA and BGA Thermal Cycle Performance and Eliminates Underfill
Global manufacturing solutions provider

Reflow Oven