Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Is anyone has experience on problems with press-fit on Ni/Au...
- Apr 18, 2002
by
General comments are:
* First place I would look is the sup...
- Apr 18, 2002
by
davef
I have only seem problems so I would suggest you don't do it...
- Apr 29, 2002
by
Hi,
we do Sn plated I/O pinning insertion into Ni/Au thru...
- Apr 29, 2002
by
ianchan