Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 6989
We have a customer transitioning slowly to lead free due to ... - Mar 06, 2006 by Craig
Craig - You should not use the leaded parts, as you are, in ... - Mar 07, 2006 by BillyD
I have to disagree with you, BillyD. If Craig searches the ... - Mar 07, 2006 by muse
muse- I agree with you. You should never mix chemistries if ... - Mar 07, 2006 by BillyD
Billy, I have to disagree with you. We inadvertently sol... - Mar 07, 2006 by
I think it has a whole lot to do with the heat applied, and ... - Mar 07, 2006 by BillyD
Craig. i spoke with a process engineer today and he told ... - Mar 07, 2006 by boomer
You have 2 groups giving us 'evidence' here: 1. the researc... - Mar 10, 2006 by
Hi Craig: I agree with muse. The problems almost always w... - Mar 11, 2006 by
Hi, We have been soldering lead free BGA's onto products ... - Mar 12, 2006 by Grant
The original issue was Co. does not need to go Pbfree, but ... - Mar 13, 2006 by muse