Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3489
I have read an interesting article on pip plus, where they s... - May 08, 2006 by Smartasp
Search the fine SMTnet Archives for previos discussions on s... - May 09, 2006 by davef
indium and alpha frye have preforms ... - May 09, 2006 by RDR
Yoinks. I'd look selective solder. Preforms are a pain, bu... - May 09, 2006 by
Yoinks. We'd look dispensing solder paste. Preforms are expe... - May 09, 2006 by davef
Hi I use a lot of preforms for other specific applications.... - May 12, 2006 by Slaine
Remember, the components' bodies are not going to like the e... - May 12, 2006 by Rob
Ha ha Chunks. No w you see, we are against you. Thanks you ... - May 14, 2006 by Dr Shocker
Thank you guys for all the info. Sure have a beter idea now.... - May 15, 2006 by
M'kay, "I" see now. Thanks for straightening me out on the ... - May 15, 2006 by