Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2583
Hi, We are about to change our wave over to lead free sol... - May 18, 2006 by
What is your bath made out of? ... - May 18, 2006 by
Are you talking a tin purge here? ... - May 18, 2006 by RDR
Hi, The bath is titanium coated, and the machine is only ... - May 18, 2006 by Grant
We did a tin bath on ours but it was provided for free by Ni... - May 18, 2006 by adlsmt
I don't have any experinence with this, but my concern is th... - May 18, 2006 by Bman
Hi, The tin flush is a good idea, and better than the sup... - May 18, 2006 by Grant
Hi, One other thing, and it's weird to be replying to mys... - May 18, 2006 by Grant
"Solder alloy compositions are numerous but the most importa... - May 18, 2006 by
Grant