Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 2289
Hi, We have a 5 zone oven and we use a RTS Profile. Our ... - May 26, 2006 by
the oven is convection reflow ... - May 26, 2006 by
Here are settings for a Vitronics SMR500 oven for Indium Cor... - May 26, 2006 by PeteC
Thanks Guys. ... - May 29, 2006 by
dave