Topside Heat on Board | 29 May, 2006

All,

What method does everyone use for measuring the heat on the topside of the board in a Wave- we are currently using temp stickers. If the Flux is activated at between 110-120 degrees Celcius does this mean that the topside should read around 90 degrees?

Marc

reply »

#41888

Topside Heat on Board | 30 May, 2006

Temp stickers work fine but a temp profiler gives you more useful data. The topside temp depends on the type of flux you use Look at the flux spec sheet or ask your flux supplier.

Patrick

reply »

#41889

Topside Heat on Board | 30 May, 2006

Howdy Marc, Check with your flux vendor, they should have a data sheet with what you need. Baring a wave rider or other profiler, I use a laser thermometer (They're cheap.)and It gets me close to where I need to be on our assemblies. I usually check after preheat 1 and after preheat 2. For example I use Kester 920CXF and they recomend a top side temp of between 180F-220F. Hope this helps. Jay

reply »

Vince Whipple

#41957

Topside Heat on Board | 2 June, 2006

Marc, Topside temperature is one of the most critical parameters for a successful solder process. Temp stickers are OK to use but won�t tell you the temperature in tight areas. The temp gun like Jay suggested is what I use as a quick indicator. (Raytek MT is the one I have and cost me about $50)

The temp that the flux manufacturer is referencing is a reading taken just before the board makes contact with the solder. So your 110-120 degrees is just before the solder contact and the reading is on the top side.

As Patrick said, the best tool to use is a profiler. It works by attaching thermocouples to your board at multiple areas and then gives you a picture of temp over time for each location. The following is a link that shows the profile output from a profiler:

http://www.ecd.com/emfg/instruments/mole/mole_scan.asp

(or you can get an idea as to delta t by using the 2 readings like Jay does and then doing the math. If you have SMT, get a profiler though.) In our training classes we recommend the use of a profiler regularly and the temp gun for quick checks. And I can�t stress enough how important the temperature is to a successful process; especially for a no clean process!

Good Luck, Vince Whipple, Sono-Tek.