Hi, We have spent the day trying to profile our Vitroncis... - Jun 09, 2006 by Grant
I think You should try to do the Delta X test, because there... - Jun 09, 2006 by
I am sorry, but I hope No hard feelings? :) As for an answe... - Jun 09, 2006 by
Hi, Very funny, and I feel so much better not because of ... - Jun 09, 2006 by Grant
Dont't bother to answer real idiots! I can relate to a si... - Jun 10, 2006 by Mika
Yeehaa! there little doggies, y'all just got to mine that th... - Jun 10, 2006 by
Grant, I beleive your problem may lie in the top side hea... - Jun 11, 2006 by
Flux: Getting enough- is the spray fluxer getting good throu... - Jun 12, 2006 by
Hi Grant, Boy, how do I say this - I might have to agree ... - Jun 12, 2006 by
Hi Grant, You definitely have a pre-heat problem and not ... - Jun 12, 2006 by Patrick Bruneel
My brother-in-law is a DDS and I trust him. We had some pro... - Jun 12, 2006 by
It's hard to believe MoonMan spends this much time typing th... - Jun 12, 2006 by
Hi, Thanks guys for all the suggestions. I am going to ch... - Jun 12, 2006 by Grant
Hi. I agree that the Soltec has weak, low-wattage prehe... - Jun 12, 2006 by
Hi, Thanks, and we are doing that today. After spending t... - Jun 12, 2006 by Grant
Hi, ok, I have a bit more info after playing further with... - Jun 13, 2006 by
Well grant just to let you know i feel your pain. I've been ... - Jun 13, 2006 by bruce
Your new problem is inadequate flux coverage. This may ... - Jun 13, 2006 by RDR
Hi, Your right guys, and we turned off the chip wave, and... - Jun 13, 2006 by Grant
Hi, Is it possible to have too much flux? Grant ... - Jun 13, 2006 by Grant
Samir's ICT guy says YES. ... - Jun 13, 2006 by
Yes it's definately possible to have too much flux. You'll s... - Jun 14, 2006 by bruce
What rpm is the Delta wave going at? (I think it was recomme... - Jun 14, 2006 by Rob
Hi, Thanks for all the help guys, and we did a bunch of t... - Jun 14, 2006 by Grant