Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 6262
Hello, Has anyone had issues with voiding while using Imm S... - Jun 22, 2006 by
do you mean microvoids or macrovoids?? ... - Jun 22, 2006 by Amol Kane
First, we expect voiding in imm silver to be similar to ENIG... - Jun 22, 2006 by davef
Some amount of voiding was always seen on sites where solder... - Jun 23, 2006 by
It does make you think the immersion coating is causing the ... - Jun 26, 2006 by davef
We saw this condition over 3 years ago. It sometimes is ca... - Jun 26, 2006 by
Yes it does seem like a plating issue and analysis is being ... - Jun 27, 2006 by
There was a good artical on this in Assembly Magazine Octobe... - Jun 27, 2006 by
Wow, great article there mike! Thanks for digging it up for... - Jun 28, 2006 by
Good article. Would EDX analysis of the cross-section at th... - Jun 28, 2006 by
Yes, it would. That you are asking this question makes us w... - Jun 28, 2006 by davef
Gman