Most of pcb have white/black printing at bottom side of them... - Dec 27, 2006 by
Tough call without seeing the board, but here's my best gues... - Dec 28, 2006 by Steve Thomas
I know our glue looks different when applied over different ... - Dec 28, 2006 by Real Chunks
So I'm the only one that's had crappy piles of silkscreen be... - Dec 28, 2006 by Steve Thomas
i just thought that it because of difference thickness betwe... - Dec 28, 2006 by
Crappy piles? Weren't they a hard rock band in the 80's? I... - Dec 29, 2006 by Real Chunks
We had a supplier that put a [fuzzy and of variable height) ... - Jan 02, 2007 by Steve Thomas
Chalk this one up to semantics. Regardless of when you start... - Jan 02, 2007 by Steve Thomas
But that's how Purchasing is supposed to work, right? Then ... - Jan 02, 2007 by Real Chunks
Not to mention the couple hunnert they save by NOT getting a... - Jan 02, 2007 by Steve Thomas
i want to learn from u