Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3170
I have this board that we are currently having problems with... - Feb 23, 2007 by
Running the BGA first is OK. We run double sided BGA baords... - Feb 23, 2007 by Real Chunks
Hi, I believe ,do the BGA side first and then use glue from... - Mar 01, 2007 by
Hi, I believe ,do the BGA side first and then use glue from... - Mar 01, 2007 by
Run the lead free BGA side first. Then run the tin lead sid... - Mar 01, 2007 by
It sounds like something is a little off here. ROHS compati... - Mar 01, 2007 by Rob Thomas
We are using lead paste on both sides, the only reason we ne... - Mar 01, 2007 by
1) run the BGA side first. set the bottom temp lower (if you... - Mar 01, 2007 by
There is a formula that determines whether a component will ... - Mar 02, 2007 by Samir Nagheenanajar
Are you using lead free paste also? Are all the other parts ... - Mar 02, 2007 by KSimpson
Samir's correct. We've talked about this previously. Searc... - Mar 02, 2007 by davef