Hello, We are having issue with one of the customer boar... - Mar 05, 2007 by
On your ENIG thickness requirements, search the fine SMTnet ... - Mar 05, 2007 by davef
Hi Mark, Solder paste will not flow on Ni like it appears... - Mar 06, 2007 by Real Chunks
Hello, We replated the boards with new Ni and Au and the... - Mar 07, 2007 by
Well there ya go, this proves you can't engineer from your d... - Mar 07, 2007 by Real Chunks
ENig can vary in quality, but I've never seen an ENiG board ... - Mar 08, 2007 by Dirk Nuendyke
There is nothing to argue if you had found Ni above or togat... - Mar 11, 2007 by
Mark