Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 4511
Anyone knows about the top side remelting requirement for wa... - Mar 26, 2007 by
Hi Amy, 183 degrees C if it's 63/37 paste. For wave ... - Mar 26, 2007 by Real Chunks
The temperature that will melt solder holding top side SMT c... - Mar 26, 2007 by davef
Unless those vias are used for ICT or test. ... - Mar 26, 2007 by Real Chunks
Someone had a fiiiine weekend. ... - Mar 26, 2007 by Steve Thomas
I don't do wave soldering but want to see if I understand th... - Mar 26, 2007 by
Not really. Spent half of it at work. And you? Did you ha... - Mar 26, 2007 by Real Chunks
Yes, I have tested some boards, and found that most QFPs whi... - Mar 26, 2007 by
There is no "standard" or "procedure". Your customer is put... - Mar 27, 2007 by Real Chunks
Amy, One way you can drastically lower the peak temperatu... - Mar 27, 2007 by Dirk Nuendyke
Amy