Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 4304
Anyone have experience wave soldering rigid flex assemblies?... - Apr 04, 2007 by robgd3
Maybe more baking time is needed. Topside board temp too ... - Apr 04, 2007 by PeteC
Rob: How do you rework blow-holes and pin-holes? PTH plat... - Apr 04, 2007 by davef
Pete, Top-side temp might be an issue. What's the easies... - Apr 04, 2007 by robgd3
The easiest, long term cheapest, and most accurate way to ... - Apr 04, 2007 by davef
Dave, We're reworking with flux and solder. We're observ... - Apr 04, 2007 by robgd3
On finding baking recipes in the fine SMTnet Archive, your p... - Apr 05, 2007 by davef
Dave, I've seen some instances of solder as you mentioned... - Apr 05, 2007 by robgd3
Please note that pin holes and blow holes are not always def... - Apr 05, 2007 by PeteC