Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 15039
Hello All, I have been searching for the board assemblies b... - Aug 08, 2007 by BTran
There are no requirements acceptance criteria for baking of ... - Aug 09, 2007 by davef
DaveF, Our customer requirement is to comply with IPC-STD-0... - Aug 09, 2007 by BTran
Tran Since we all agree that J-001 has no baking requiremen... - Aug 10, 2007 by davef
Davef, The J Standard-001-DS(Ref. 4.9.3)does required board... - Aug 10, 2007 by BTran
Tran First, you never spoke of J-001DS in your initial post... - Aug 11, 2007 by davef
My apology for not mentioned the J-STD-001DS. I didn't mean ... - Aug 14, 2007 by BTran
Just talking off the top of my head, I'd guess that greater ... - Aug 14, 2007 by davef
Here is what you need to do if you can, Since you want... - Aug 16, 2007 by RDR
My small reflow oven doesn't have the rails (only metal mesh... - Aug 17, 2007 by BTran
Here's how to double reflow your QFP: * Reflow the first si... - Aug 18, 2007 by davef