Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 7178
Hello What type of error proofing methods are you guys... - Oct 04, 2007 by Pitbull
Paint no-lead stuff green and carry a big stick. ... - Oct 04, 2007 by Hussman
Everything for a lead free job is labeled with green lead fr... - Oct 04, 2007 by jdengler
Use dedicated stencils & gold or green squeegee holders ... - Oct 04, 2007 by Mike007
Yeah, but when the operator drops regular solder bars into y... - Oct 05, 2007 by FD
Thanks for the replies. We have been doing the same thing. T... - Oct 05, 2007 by Pitbull
We have done the Green Framed Stencils for an added $50.00 p... - Oct 10, 2007 by pete
Thank you- my point exactly and it starts in SMT- operators ... - Oct 11, 2007 by mparker
As a CM, how can you change the customer's base PC Board mat... - Oct 11, 2007 by pete
Michael We know you're just trying to have fun by getting... - Oct 12, 2007 by davef
All- good points and to be clear not all is in fun and jest.... - Oct 12, 2007 by mparker
The only sophisticated customer I have is 100% ROHS and actu... - Oct 12, 2007 by mparker
> I'm a > CM- high mix, low to medium volumes. No st... - Oct 17, 2007 by Stephen
Yes Stephen and has been discussed in a thread before. Ch... - Oct 17, 2007 by Patrick Bruneel
Certainly could be true - so do we keep producing with toxic... - Oct 17, 2007 by mparker
The true cause and effects of the other pollutants have been... - Oct 17, 2007 by Steve Thomas