Yea, I'm still here.....sigh. Got bridging problems. T... - Feb 20, 2008 by Paul M.
Tented vias have solved problems for me in the past, but nev... - Feb 20, 2008 by Steve Thomas
That is a correct assumption Doug. ... - Feb 21, 2008 by Paul M.
KRIKIES! tenting WILL inhibit solder flow through the top-s... - Feb 21, 2008 by Chim Richalds
If the vias are large and don't always tent, you can have yo... - Feb 21, 2008 by Flipit
if you are not using them for test points or want them fille... - Feb 21, 2008 by Dave
Are you using nocleans, especially when you get to SMT? Y... - Feb 22, 2008 by SteveK
Steve, Trying to keep wave solder from coming up the via'... - Feb 22, 2008 by Paul M.
Rather than having the artwork cover the via as with tenting... - Feb 25, 2008 by SteveK