Can anyone recommend a conformal coating that can be applied... - Apr 30, 2008 by John Sims
Paraffin wax. Before you laugh, check it out. ... - Apr 30, 2008 by Real Chunks
I believe Humiseal (and others) makes some water based coat... - Apr 30, 2008 by MikeS
Humiseal has no-VOC coatings Acrylic and Urethane on offer, ... - May 02, 2008 by josh