Hi all, What should the typical gold thickness be on ENIG... - Jul 10, 2008 by aj
Search the fine SMTnet Archives to find threads like: ... - Jul 10, 2008 by davef
Thanks Dave, IPC-6012 states min at 0.05um. Has this b... - Jul 11, 2008 by aj
0.05 um => 2 uinch, right? Here is the revision level for... - Jul 11, 2008 by davef
Hi Dave, Yes that is correct. I had a XRF carried out ... - Jul 11, 2008 by aj
Hi Aj, Recommended Immersion gold thickness would be 3-5 ... - Jul 15, 2008 by BoardHouse
Please look up ... - Jul 28, 2008 by Mark