We are in the process of preparing for a new board that requ... - Aug 18, 2008 by floydf
Stencil apertures are cut to deposit solderpaste onto the an... - Aug 18, 2008 by PeteC
No I was actually thinking more on the lines of this. ... - Aug 18, 2008 by Doug Philbrick
We do it all the time for air pressure reasons. Use a 6 mil... - Aug 18, 2008 by Real Chunks
Real Chunks, Does "aperture opening 100% same size as the vi... - Aug 18, 2008 by floydf
Oops, I thought it was for components- not filling via holes... - Aug 18, 2008 by PeteC
Open the same size as the via's anular ring. Any slight off... - Aug 18, 2008 by Real Chunks
Volume of paste = 2X volume of the hole Questions are: *... - Aug 18, 2008 by davef