I had a vendor change thier lead finish from tin/lead to a S... - Sep 16, 2008 by Trynders
Well, typical content of Pb in Sn/Pb polating is a few perce... - Sep 16, 2008 by Vlad
Yes, this scenario is fine. However, BGAs are a different s... - Sep 16, 2008 by Dirk Nuendyke
Well, as we are talking about lead finish, I don't think the... - Sep 16, 2008 by Vlad
Vlad, yes, he made no mention of a BGA, but I thought I'd ju... - Sep 16, 2008 by Dirk Nuendyke
Thanks for the response! I thought is was odd the component ... - Sep 16, 2008 by Trynders
Even BGA may be no braner if it's done properly :-) I had a ... - Sep 16, 2008 by Vlad
There is one thing you should keep in mind, though. It's bet... - Sep 17, 2008 by Vlad