Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 3851
Hi I am looking for informations/specs about graphite/car... - Feb 26, 2009 by GSx
There is no IPC specification on carbon ink. Consider tal... - Mar 05, 2009 by davef
Thank you so much Dave, by having different lots of PCB r... - Mar 11, 2009 by GSx
Hi GSX, just and FYI on why you are seeing a difference p... - Mar 13, 2009 by BoardHouse