Board delaminated after reflow - see attached picture. Does ... - Apr 07, 2009 by 1036
We don't view this as "board delamination." It looks more li... - Apr 08, 2009 by davef
push the "bubling" and it springs back. It does not look lik... - Apr 08, 2009 by 1036
That is a delamination. It is indeed from moisture. You need... - Apr 08, 2009 by tommyttr
We had the exact same problem in early stages of lead-free. ... - Apr 08, 2009 by SWAG
Hi, Need a little more info, 1) this board is definite... - Apr 08, 2009 by BoardHouse
2) STD FR4 material with HASL finish, 4 layer board. Reflowe... - Apr 08, 2009 by 1036
The things to ask your board supplier would be: 1) Was th... - Apr 08, 2009 by BoardHouse
We have seen this exact same problem. Our vendor agreed it w... - Apr 16, 2009 by Cross