Hi, Our SMT line has placement capacity of 80K cph, but o... - Sep 21, 2009 by rodnas
Why not: * Stencil print glue? * Stencil print the majorit... - Sep 21, 2009 by davef
We don't have any experience printing glue. Our equipment su... - Sep 21, 2009 by rodnas
What babies!!!! Sure, give it a try. * Stencil material: me... - Sep 21, 2009 by davef
Anytime we use a glue/wave solder process we print the adhes... - Sep 21, 2009 by dontfeedphils
The only time I ever saw problems with stenciling glue was w... - Sep 22, 2009 by Stephen
I think I forgot to mention a little detail here: our boards... - Sep 22, 2009 by rodnas
Yes, after you move SMT to before PTH like everyone else. ... - Sep 23, 2009 by Stephen
Santiago can still maintain his current PTH, SMT, Reflow, Gl... - Sep 23, 2009 by davef
Thanks to all for the great replies. I guess we'll buy a ste... - Sep 23, 2009 by rodnas
We apply temporary solder mask off line, using a programmabl... - Sep 23, 2009 by davef
Those articles are talking about screening before PTH placem... - Sep 24, 2009 by Stephen
Both of the articles talk about pockets cut in the contact s... - Sep 24, 2009 by davef