I work for a CEM. We are having some quality issues with som... - Oct 27, 2009 by Julie
Top picture: We're not wild about the 'poor registration,' t... - Oct 27, 2009 by davef
solderresist has a big offset? ... - Oct 28, 2009 by Loco
I don't like these boards for a couple different reasons. ... - Oct 28, 2009 by Julie
I agree with you. Personally, I would either return them an... - Oct 28, 2009 by SteveO
The top picture probably won't run. You have black soldermas... - Oct 29, 2009 by Comatose
Hi, I see a huge solder mask shift on chip comp pads. This ... - Oct 30, 2009 by Richard
Just my opinion: Top pic - Solder mask registration WAY t... - Nov 01, 2009 by isd.jww
Hello Julie Yr supplier is saying that these boards meet... - Nov 01, 2009 by Jeong Ju-young
Hi Julie, My opinion is that the top board would not pass... - Nov 01, 2009 by BoardHouse
Base on the top picture condition, seems like the boards con... - Nov 02, 2009 by Umar
Umar - the boards are not assembled - so Solder splash is no... - Nov 02, 2009 by BoardHouse
Davef, you really make me laugh!!! pretty funny sarcastic wa... - Nov 03, 2009 by Manuel
Has anyone ever done a tape test to see if the solder resist... - Nov 03, 2009 by Josh
Solder Mask Adhesion Pull Test Tape List IPC-TM-650 Test Me... - Nov 03, 2009 by davef
Thank you, Manuel ... - Nov 03, 2009 by davef