Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 5901
We are using Humiseal 1B31 and polyester dots for masking. W... - Feb 25, 2010 by pbrown
My guess would be that the adhesive used on the dots contain... - Feb 25, 2010 by jdumont
It sounds like your poly dots are secreting something that a... - Feb 25, 2010 by davef
If I had to guess I'd say they're using a silicone based adh... - Feb 26, 2010 by kpm
Your masking dots are a silicone adhesive. Contact the suppl... - Feb 26, 2010 by MGL
Hey its probably the silicone adhesive ... - Feb 26, 2010 by jdumont
sorry jdumont I didn't see your post until after I posted mi... - Feb 26, 2010 by kpm
No problem just busting, trying to keep the mood light! ... - Mar 01, 2010 by jdumont
Hey....I think it might be the silicone adhesive! LOL Yeah... - Mar 01, 2010 by Lou