We are looking at buying a new (or used) oven for low-mid vo... - Apr 16, 2010 by Shawn Vike
I have owned Vitronics, BTU, ETS, & Heller. The Vitronics w... - Apr 16, 2010 by Flipit
As a solder paste supplier I have profiled lots of different... - Apr 17, 2010 by Graham
I personally would be wary of heller1707EXL and as I have m... - Apr 17, 2010 by josh
Thanks, that is the problem that I have with my current oven... - Apr 19, 2010 by Shawn Vike
when I profile a customers oven / pcb I always try a check t... - Apr 23, 2010 by Graham
Graham, When performing such a temperature variation test... - Apr 23, 2010 by SteveO
I always fix thermocouples to pcb pads across its width. The... - Apr 26, 2010 by Graham
> when I profile a customers oven / pcb I always > t... - Apr 28, 2010 by josh
Another Brand worth checking out is Rehm, pretty good rep in... - Apr 28, 2010 by josh