Is there any way to measure the copper oxide thickness on th... - Aug 30, 2010 by James
Sure, you should be able to measure the copper oxide thickne... - Aug 30, 2010 by davef
Dave, Thanks for the reply. I didn't realize that you wo... - Aug 30, 2010 by James
Dave can you be more specific on this? I will be interested ... - Sep 03, 2010 by Nicoleta
James, Are you referring to oxidation caused on outer laye... - Sep 03, 2010 by sachu_70
SERA testing (sequential electrochemical reduction analysis)... - Sep 08, 2010 by blnorman