OGER 4003C bounding to Aluminum
I am hoping someone might have the solution to my problem I have the following PCB: RO4003 Thickness: .2mm Layer: top single/ bottom ground plane Finish: silver top and bottom .2um Size: 3mmx6mm
I need to bound/ground this to an aluminum carrier with silver finish.
I tried tinning the ground plane of the PCB and the aluminum carrier with RoHS solder Then using a hot plate I increase the temp of the aluminum carrier Applied flux to the PCB ground plate And applied the pcb to the aluminum carrier Using a weighted jib I would hold the pcb on top of the aluminum carrier and cooled it down at room temperature.
The problem is.. its not a great process ..
Is there a better way to do this job ?
reply »