Flexible substrate coated by PR+, found many open trace. The... - Feb 12, 2011 by lafir
lafir
#63745
Photoresist+ Peel of Cu surface | 12 February, 2011
Flexible substrate coated by PR+, found many open trace. The Photo resist peels off from CU surface randomly creating open circuit during devolopement. Any ideas???
reply »