Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 8404
Hi, We are using ws488 sn100c paste. Anyone have a pr... - Mar 30, 2011 by gaz
While you're waiting, consider giving your paste manufacture... - Mar 31, 2011 by robgd3
starting point with zone settings would be, 100 / 160 / 200 ... - Apr 01, 2011 by Graham
This VIP70 has thermocouple inputs, so I'm hoping that's a... - Apr 04, 2011 by gaz
one of my customers with a BTU VIP 70 has the following sett... - Apr 05, 2011 by Graham
That's very helpful, and much appreciated. I know it's ... - Apr 05, 2011 by gaz
It is one of our pastes...Almit LFM48 W TM-HP, a high reliab... - Apr 05, 2011 by Graham
We are not having any real issues. I am just first setting... - Apr 05, 2011 by gaz
Almit are specialists in formulating fluxes for pastes and w... - Apr 06, 2011 by Graham
ok, thanks very much for your help. ... - Apr 06, 2011 by gaz