Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 4720
Here's the scenario: PCB Plating: Lead free HASL, Sn100C... - Dec 13, 2011 by Dirk Nuendyke
Contaminating lead-free solder connections with lead is gene... - Dec 13, 2011 by davef
DaveF, That's correct. This assembly is plain old tin-le... - Dec 13, 2011 by Dirk Nuendyke
There should not be a problem we have done this. If you are ... - Dec 13, 2011 by KaHrpr