My circuit board contains 11 x 11 matrix 1mm pitch BGA, The ... - Jun 17, 2013 by saravanan
You have not mentioned exactly how the BGA was reflowed onto... - Jun 17, 2013 by Hegemon
Hi, the BGA and/or the PCB may be warping excessively during... - Aug 30, 2013 by smtgs02jrt
One of our PCB for high reliability application is having 2 ... - Oct 21, 2013 by saravanan
The first picture shows an issue. Note that the vias adjace... - Oct 21, 2013 by Hegemon
In continuation of the thread, attached 2d & 3d x-ray pictur... - Nov 07, 2013 by saravanan
1st X-Ray looks pretty good. One instance of what looks lik... - Nov 07, 2013 by Hegemon