I have a CM project that is a single sided pcb (not plated t... - Jul 17, 2013 by ProcEng1
Sure. Section 7.4 covers unsupported holes, and defines the... - Jul 17, 2013 by robgd3
argh! the 6 ends of the resistors soldered to another though... - Jul 17, 2013 by EricR
The parts are just soldered to the pads. There isn't anothe... - Jul 17, 2013 by ProcEng1
Everything in 7.4 shows the clinch and fillet on the other s... - Jul 17, 2013 by ProcEng1
It's what the customer wants. remember the customer is alway... - Jul 17, 2013 by SweetOldBob