Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 5187
Hola... I'm in the middle of a project to reduce assembly... - Jun 09, 2014 by Jorge_Quijano
Your bottom-side joints look deficient in solder. It appear... - Jun 10, 2014 by Reese
It is very hard to say by looking at picture(solder joint qu... - Jun 10, 2014 by Daxa
this is a Class II product. If I increase the openings...... - Jun 10, 2014 by Jorge_Quijano
Probably not considering you have ample volume left on your ... - Jun 10, 2014 by Reese
What you need here is a double print process. You should hav... - Jun 12, 2014 by Evtimov
No, is will not create random solder balls. I have experienc... - Jun 12, 2014 by Daxa
Update 6/12 After solder preform (SAC303 0603) I did not ... - Jun 12, 2014 by Jorge_Quijano
Just thought it may be helpful, my FREE 100 page ebook on Pi... - Nov 09, 2014 by Bob Willis
Hola Bob, in fact I made the proposal for the PIHR just af... - Nov 10, 2014 by Jorge_Quijano