Hi all, I'm having some troubles while trying to set up a... - Dec 26, 2016 by Luciano
Dear Pro, Pls, increase temperature up to 255ºC and consi... - Dec 27, 2016 by anhsang38
Thanks for your advice. I've tried setting the temperatur... - Dec 27, 2016 by Luciano
Dear Pro, I want to confirm with you about conveyor speed... - Dec 27, 2016 by anhsang38
Hello, Sorry for the mistake. The speed is 1m/min. We ... - Dec 27, 2016 by Luciano
Dear pro, Could you show the solder's profile. ... - Dec 27, 2016 by anhsang38
Dear Anshang38, I actually don't have a profiler in order... - Dec 28, 2016 by Luciano
Dear Pro, Pls, try to get solder's profile from solder su... - Dec 28, 2016 by anhsang38
I would cut a piece of cardboard to the same dimensions as y... - Dec 29, 2016 by SuMoTe
Luciano, It looks you have no flux there. Please flux one... - Dec 29, 2016 by Evtimov
Thanks Anshang38 I'll try and get a profiler. ... - Dec 29, 2016 by Luciano
Thanks Evtimov, The flux is brand new and the amount of f... - Dec 29, 2016 by Luciano
Thanks SuMoTe, I've already tried fluxing various boards ... - Dec 29, 2016 by Luciano
First profilers are expensive and you can use temperature do... - Dec 30, 2016 by SweetOldBob