Hello I have the problem with selective soldering on the ro... - Jun 20, 2017 by ranap121212
I would start with checking the flux amount and trace and th... - Jun 21, 2017 by Evtimov
but we do not have laminate preheating on robots. There is n... - Jun 21, 2017 by ranap121212
Try baking the boards; you may have a moisture problem. ... - Jun 21, 2017 by mac5
Are you using nitrogen in your soldering process? ... - Jun 22, 2017 by CAPSE
There are several different technologies in the industry tod... - Jun 22, 2017 by SolderingPRO
Thanks from your answer. A few days ago the supplier told me... - Jun 24, 2017 by ranap121212
@Capse, No but the machine has such a construction, I can no... - Jun 24, 2017 by ranap121212
If N2 is not an option, the cut wire feeder or drilled wire ... - Jun 26, 2017 by CAPSE