Hi, I must change our current terrible foam fluxer unit used... - Nov 16, 2017 by andras
Water soluble fluxes can be highly corrosive. Make sure that... - Nov 16, 2017 by Jandon
We installed a SonoFlux ultrasonic spray fluxer, replacing t... - Nov 16, 2017 by charliem
SonFlux EZ is not suitable for water SOLUBLE flux. SonoFlux ... - Nov 16, 2017 by Jandon
It looks SF's price level breaks the bank :( @charliem: i... - Nov 17, 2017 by andras
What formula of flux are you foaming with? I am looking for... - Feb 08, 2018 by ProcEng1
Hi, We are currently using Alfa EF-2210, that is a good wat... - Feb 08, 2018 by andras
yes but you were using a flux foamer. What flux did you use... - Feb 08, 2018 by ProcEng1
Bought spray fluxer unit extension to our machine ;) AFAI... - Feb 08, 2018 by andras
So you were never using the foamer in the machine? ... - Feb 08, 2018 by ProcEng1
Yes we used it with EF-2210, but it is a pain... not really ... - Feb 08, 2018 by andras
trying to stick with water based, yes. ... - Feb 08, 2018 by ProcEng1
I think it is better to forget foam fluxer in this case ... - Feb 09, 2018 by andras
Nope. I prefer foam. ... - Feb 09, 2018 by ProcEng1