Printed Circuit Board Assembly & PCB Design Forum
SMT electronics assembly manufacturing forum.
Views: 4617
Hi experts, I would like to ask to the forum if you could d... - May 21, 2018 by Diego
How old is the stencil and how many cycles does it have ... - May 21, 2018 by KaHrpr
Honestly, I wonder the same. Is it Age the only variable to... - May 21, 2018 by Diego
there are numerous factors: -stencil age -stencil finish... - May 22, 2018 by bukas
metal blades scraping against a metal foil; do it enough tim... - May 22, 2018 by dwl
This is caused by usage. Excessive squeegee pressure can ma... - May 22, 2018 by Sr. Tech
Those patterns are either: a) the stencil has recieved some ... - May 23, 2018 by Transition Automation
Bottom line....if you have an SPI machine, that's the judge ... - May 24, 2018 by Sr. Tech
Thank you all guys. I appreciate all your help. I am runni... - May 30, 2018 by Diego
Diego, In my opinion you are wasting your time testing. S... - May 31, 2018 by Sr. Tech